Epoxy resin reacted with methacrylic acid to form epoxy ester. Terminal double bonds cure with peroxide. strong acid/alkali and solvent resistance.
Room temperature cure, gel time 20-40min; post-cure 80°C/2h increases crosslink density.
Glass-flake mortar used for swimming pool, desulfurization tank lining, pH 2-12 resistant, lining service life ≥10 years.